IN625 nickel-chromium superalloy Powder

CMI In625 is a solution-hardened nickel-based superalloy. The addition of niobium, in combination with molybdenum, gives high strength and toughness even in the annealed condition.
In 625 is particularly suitable for applications demanding excellent tensile, creep strength.


Renowned for high strength across a broad temperature range, outstanding corrosion resistance, and excellent processability.


Equivalent materials: UNS N06625, NC22DNb, AMS7001 (chemical composition)

    Product Details

    Morphology Spherical, irregular
    Particles sizes 0-20um,15-45um,15-53 μm,45-106um, 53-150um
    Powder Available for • Additive Manufacturing (AM)
    • Metal Injection Moulding (MIM)
    Laser Cladding

    Chemical Composition

    CHEMICAL COMPOSITION WT%
    Ni Fe Cr Nb Mo Ti Co
    ≥58.0 ≤5.0 20.0-23.0 3.16-4.15 8.0-10.0 ≤0.4 ≤ 1.0
    Al Mn Si C P S
    ≤0.4 ≤0.5 ≤0.5 ≤0.1 ≤0.015 ≤ 0.015

    Material properties


    Very high corrosion and oxidation resistance at high temperatures
    Non-magnetic
    High strength
    High fatigue strength in seawater
    Excellent welding characteristics
    Excellent fabrication properties

    Applications

     

    Typical areas of use include hydraulic systems, heat exchangers and high-temperature applications, high-temperature aerospace, chemical process industry, such as to manufacture engine casings, guide vanes, mounting edges and barrels, fuel manifolds, and other components.